US US4725390A
A process for making ceramic spheriods by mixing and converting spheroids, with the aid of water, raw materials of 50-99.8 parts by weight mineral particulate (e.g. blend of orthoclase, nepheline, hornblende and diopside) which particulate includes at least one mineral having chemically bound water or sulphur in a form which is not substantially water soluble and in amounts sufficient to yield 0.5 to 5 weight percent water or 0.04 to 2 weight percent sulphur in the total mass; 0.1 to 50 parts by weight silicon carbide; and 0.1 to 15 parts binder. The wet spheroids are dried and the dry spheroids are fired in contact with a parting agent (e.g. aluminum oxide) for a sufficiently long time to form a shell containing parting agent on the ceramic mineral having a fired density of less than about 2.9 grams per cubic centimeter when fired above 1,100 DEG C. The binder is typically bentonite clay.
A document turning up in a search is not the same as a document that anticipates your claims. Our registered Patent Agents read the claims, not just the abstract, and tell you where you still have room.
Protect Your InventionBibliographic data via the European Patent Office's Open Patent Services (DOCDB) . Republished here for research and prior-art review. This page is not legal advice, and its presence in our index says nothing about the validity or enforceability of the document. For the Indian legal position (status, oppositions, renewals), see InPASS.